FilamentMatch

Material profile · enclosure strongly recommended

PA (Nylon)

Use it for: gears, bushings, living hinges, snap-fits that flex repeatedly.

nozzle 250270°Cbed 7090°Cdrying: critical

PA (Nylon) · slicer settings

PA (Nylon) print settings table
Nozzle temperature250270°C
Bed temperature7090°C
EnclosureStrongly recommended
Hardened nozzleNot needed
DryingCritical — always dry before printing

Strengths & weaknesses

  • Strengths: wear-resistant, self-lubricating, fatigue-tough — gears and hinges love it.
  • Weaknesses: drinks moisture out of the air; drying is non-negotiable, warps when wet.
  • Use it for: gears, bushings, living hinges, snap-fits that flex repeatedly.

Which printers print PA (Nylon) clean?

Verdicts below come from the documented compatibility rules — bed and hotend ceilings, enclosure, and nozzle hardness — applied identically to all 9 printers in the database. 3 print it clean, 6 need mods.

FAQ

What temperature should I print PA (Nylon) at?

Nozzle 250–270°C, bed 70–90°C. Start mid-range and tune with a temperature tower — exact sweet spots vary by brand and color.

Does PA (Nylon) need an enclosure?

An enclosure is strongly recommended for PA (Nylon). It will print on a well-tuned open machine in still indoor air, but a heated chamber dramatically improves layer adhesion and dimensional stability — and reduces warping on larger parts.

Does PA (Nylon) need drying?

Drying is critical for PA (Nylon). It absorbs moisture from the air within hours of opening; wet filament prints with popping, stringing, weak layers, and a rough surface. Dry it before every session and keep it in a dryer or dry box while printing.